Gary and friends, I called and spoke with a very helpful, friendly Steve G yesterday.

I was surprised to hear that after he has his booster halves polished to remove any pits
that he glass beads with a fine grit/grade of glass (?) BEFORE the Yellow Zinc plating.

Evidently if you zinc plate over the polished metal, the results are too shiny, not correct.

My booster halves/pieces are not "pitted" but only surface rusted. I'm wanting to glass bead the surface rust and then run booster half(s) thru a shaker machine....This
will be an experiment to see how I can condition the metal surface before plating..........
__________________
Chuck Sharin
[email protected]
Auburn,WA (30 miles South of Seattle)
70 Camaro R/S Z-28, L-78, R/S SS
69 Camaro COPO "recreation"
Reply With Quote
Reply


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT. The time now is 12:15 PM.


Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2025, vBulletin Solutions Inc.

O Garage vBulletin Plugins by Drive Thru Online, Inc.