Jeff is correct. I just cleaned up some survivor Chevelle backing plates and the galvanzing is very evident.

Sam, the reason for not using todays galvanizing process (correct me if I am wrong anybody) is due to a cold galvanizing vs hot. Todays gavanizing is much courser that was done orignally. As Micky stated, it is much better to zinc them and dull them down a touch.