Chuck,

I had my hood hinges replated with the correct zinc phosphate 4 years ago. The plater suggested that I put WD40 on them (as well as the springs) once a year to keep them from rusting. They still look as good as the day I had them done and have zero rust. For my hood catch (the part that bolts on the hood) I painted that and it's almost a perfect match with no maintenance necessary except for a little white lithium grease on the end.
__________________
Jim
Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT. The time now is 10:32 AM.


Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2025, vBulletin Solutions Inc.

O Garage vBulletin Plugins by Drive Thru Online, Inc.