Default Re: cad / zinc /galvanizing on certain parts

Jeff is correct. I just cleaned up some survivor Chevelle backing plates and the galvanzing is very evident.

Sam, the reason for not using todays galvanizing process (correct me if I am wrong anybody) is due to a cold galvanizing vs hot. Todays gavanizing is much courser that was done orignally. As Micky stated, it is much better to zinc them and dull them down a touch.
Rick
__________________
Rick Nelson
Musclecar Restoration and Design, Inc (retired)
www.musclecarrestorationanddesign.com
https://www.youtube.com/watch?v=62r-6vgk2_8
specialized in (only real) LS6 Chevelle restorations
Reply With Quote
 

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT. The time now is 12:02 PM.


Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2025, vBulletin Solutions Inc.

O Garage vBulletin Plugins by Drive Thru Online, Inc.