Re: ZL1 block found
Having done quite a bit of Aluminum welding, the entire Block must be preheated (600 deg F) or so before welding. Aluminum has a fairly high coeffecient of expansion so when the weld cools, it contracts, causing stress and warpage. Also, preheating allows better penetration of the weld due to less heat draw into the block. The Aluminum alloy will make a difference as well, cleanliness, etc. Welding on die cast parts is difficult because of the higher silicon content and general imputities in the Aluminum.
It can be done with the right steps.