I'm a proponent of Palmetto's chemicals. Using their MANGANESE Phosphate solution, I feel its dead on correct for fasteners, shift rods, and misc other parts. The ZINC Phosphate is applicable for Hood hinges, hood latch and the like.
I use Colman Camp fuel (bought at Walmart) in the one gallon can for a rinse. Can says it contains a rust inhibitor as well. After drying off on shop towel, I then spray and "massage" with BoeShield T-9 (order from www.BoatersDiscountWorld.com). Boesheild has been tested by Yachting Magazine for salt spray corrosion and is FAR, FAR superior to WD-40 and the others...........
I can go on and on with MANGANESE Phosphate coating for the two of you left reading, but who cares????????????

I Love ya man,

Chuck S