Default Re: cad plating versus zinc plating

This company http://www.palmetto-omnitek.com/Palmetto/index.htm sells phosphateing chemicals for the do it yourselfer....The MANGANESE(Iron) phosphate is used for fasteners and many brkts whereas the ZINC phosphate is used for hood hinges, hood catch etc.....I have seen the results firsthand and its absolutely first class......Chuck S