Not familiar with Delfleet but if it's a polyurethane and within the same line of paint, you're good to go. This is a great method to achieve you're desired gloss. Remember to shoot a test panel, then let it cure for at least an hour to gauge the true gloss.
Using flattening agent is always a chore and results are tough to duplicate. SEM gives you 1 result, no variants, having 2 parts to custom mix gives you full control.
|